dc.contributor.author |
Mutombo, K
|
|
dc.contributor.author |
Du Toit, M
|
|
dc.date.accessioned |
2010-08-31T08:08:20Z |
|
dc.date.available |
2010-08-31T08:08:20Z |
|
dc.date.issued |
2010-08-31 |
|
dc.identifier.citation |
Mutombo, K, Du Toit, M. 2010.Fatigue performance of matching and dissimilar joints in Aluminium Alloys 5083-H111 and 6061-T651 after fully automatic pulsed GAMW using ER5356 filler wire. CSIR 3rd biennial conference: 2010 science real and, relevant, CSIR International Convention Center, Pretoria, South Africa, 30 August-1 September 2010, pp 8 |
en |
dc.identifier.uri |
http://hdl.handle.net/10204/4239
|
|
dc.description |
CSIR 3rd biennial conference: 2010 science real and, relevant, CSIR International Convention Center, Pretoria, South Africa, 30 August-1 September 2010. |
en |
dc.description.abstract |
The tensile strength and fatigue properties of Al5083-H111 welded with aluminium-magnesium alloyed ER5356 filler wire appeared similar to those of the base metal. This joint failed in the weld metal as a result of a slight reduction in hardness in the vicinity of the fusion line. However, the joints of Al6061-T651 similar and the dissimilar welds with Al5083-H111 displayed significant reduced strength and fatigue life due to lower hardness and tensile strength in the heat-affected zone. |
en |
dc.language.iso |
en |
en |
dc.publisher |
CSIR |
en |
dc.subject |
Aluminium alloy 5083-H111 |
en |
dc.subject |
6061-T651 |
en |
dc.subject |
Pulsed gas metal arc welding |
en |
dc.subject |
ER5356 filler wire |
en |
dc.subject |
Dissimilar welds |
en |
dc.subject |
Tensile properties |
en |
dc.subject |
Fatigue properties |
en |
dc.subject |
CSIR Conference 2010 |
en |
dc.title |
Fatigue performance of matching and dissimilar joints in aluminium alloys 5083-H111 and 6061-T651 after fully automatic pulsed GAMW using ER5356 filler wire |
en |
dc.type |
Conference Presentation |
en |
dc.identifier.apacitation |
Mutombo, K., & Du Toit, M. (2010). Fatigue performance of matching and dissimilar joints in aluminium alloys 5083-H111 and 6061-T651 after fully automatic pulsed GAMW using ER5356 filler wire. CSIR. http://hdl.handle.net/10204/4239 |
en_ZA |
dc.identifier.chicagocitation |
Mutombo, K, and M Du Toit. "Fatigue performance of matching and dissimilar joints in aluminium alloys 5083-H111 and 6061-T651 after fully automatic pulsed GAMW using ER5356 filler wire." (2010): http://hdl.handle.net/10204/4239 |
en_ZA |
dc.identifier.vancouvercitation |
Mutombo K, Du Toit M, Fatigue performance of matching and dissimilar joints in aluminium alloys 5083-H111 and 6061-T651 after fully automatic pulsed GAMW using ER5356 filler wire; CSIR; 2010. http://hdl.handle.net/10204/4239 . |
en_ZA |
dc.identifier.ris |
TY - Conference Presentation
AU - Mutombo, K
AU - Du Toit, M
AB - The tensile strength and fatigue properties of Al5083-H111 welded with aluminium-magnesium alloyed ER5356 filler wire appeared similar to those of the base metal. This joint failed in the weld metal as a result of a slight reduction in hardness in the vicinity of the fusion line. However, the joints of Al6061-T651 similar and the dissimilar welds with Al5083-H111 displayed significant reduced strength and fatigue life due to lower hardness and tensile strength in the heat-affected zone.
DA - 2010-08-31
DB - ResearchSpace
DP - CSIR
KW - Aluminium alloy 5083-H111
KW - 6061-T651
KW - Pulsed gas metal arc welding
KW - ER5356 filler wire
KW - Dissimilar welds
KW - Tensile properties
KW - Fatigue properties
KW - CSIR Conference 2010
LK - https://researchspace.csir.co.za
PY - 2010
T1 - Fatigue performance of matching and dissimilar joints in aluminium alloys 5083-H111 and 6061-T651 after fully automatic pulsed GAMW using ER5356 filler wire
TI - Fatigue performance of matching and dissimilar joints in aluminium alloys 5083-H111 and 6061-T651 after fully automatic pulsed GAMW using ER5356 filler wire
UR - http://hdl.handle.net/10204/4239
ER -
|
en_ZA |